2023年10月9日星期一

Slider Design

 

Things you need to know about how to design of mold slide.

Posted on : March 11, 2022 By  GREFEE


Undercuts treatment

Movement principles & design elements of diagonal bracing pin block

Undercuts treatment uses the mold opening movement and ejection force to causes the tendency of relatively motion between angle pin and slider. There are two movements to make it separate from the undercut : mold opening direction & horizontal direction. As the below pic shows:

in the pic:

β=α+2°~3°(avoid any parts contacts or blocks when group molding & reduce friction when opening molds)

α≦25°(α is the obliquity of taper pin)

L=1.5D (L is matching length)

S=T+2~3mm(S, the distance of horizontal movement of slider, T, the end product undercut

S=(L1xsina-δ)/cosα(δ – the space between taper pin and slider, normally is 0.5MM,L1is the taper pin vertical distance inside the slider)

Clamping methods & applicable situations of diagonal bracing tip

DiagramDescription
diagonal bracingSuits for situations, like thin mold and the top clamping plate and cavity plate are closed. The contact area is long and stable.
diagonal bracing1Suits for situations, like thick mold, large mold cavity.
applicable to two plate mold/three plate mold.The contact area L≧1.5D(D is diameter of diagonal bracing tip), good stability
diagonal bracing2Suits for thick mold
applicable to two plate mold/three plate mold  
contact area L≧1.5D(D is diameter of angle pin), poor stability, hard to processing
diagonal bracing3Suits for situations, like thin mold and the top plate mold and cavity plate can be separated.
Long contact area, good stability

Movement principles & design elements of pulling block

The mold opening movement of molding machine causes a tendency of relatively motion between pulling blocks and sliders.

See pic below:

in the pic above:

β=α≦25° (α – the obliquity of pulling block)

H1≧1.5W   (H1-matching distance)

S=T+2~3mm (S-distance of horizontal movement of slider, T- end product undercut)

S=H*sinα-δ/cosα(δ – the space between diagonal bracing tip and sliders, normally is 0.5MM,L1is the vertical distance of

H-vertical distance of pulling block inside the slider)

C- motion stopping surface so the pulling block form doesn’t need motion-stoping surface(no space)

Slider locking & fixing solutions

There is a huge pressure during the molding machine injection process. To avoid affecting the side and appearance(eg. burrs) of end products, we should keep the slider and core unmoved when molding machine injection. So the slider should use locking fixed method to keep it stay. normally, this part is motion-stoping block or heel.

Some common locking methods:

DiagramDescriptionDiagramDescription
diagonal bracing4The sliders are pieced together, normally used for standard products. Normally used standard products, check standard parts catalogue. Good structure and hardness.
Applicable to situations needing strong locking force.
diagonal bracing5Use insert mode to lock.
Applicable to wide sliders.
diagonal bracing6Use integrated locking mode. Good rigidity and structure. Hard to processing. Short Demolding distance. Applicable to small moldsdiagonal bracing7Use insert mode
Applicable to  wide sliders
diagonal bracing8Pulling or stopping
Poor stability
Applicable to  situations of small slider space
diagonal bracing9Are pieced together
Good rigidity
Applicable to situations of large space

Fixed methods of slider

The slider will move a certain distance in mold opening. One way to make the slider return back smoothly is to use equipment to fix it and it should be flexible and stable so that the slider will stay at where it should be. Some exceptional situations do not need fixed equipments, like left to right slider, so it is suggested to apply a fixed equipment.

 Equipment for fixing: diagramDescription
diagonal bracing10Fixing slider with spring screw, the strength of spring is 1.5-2 times the weight of slider. Applicable to upward or lateral core pulling.
diagonal bracing11Fixed by spring steel ball. Normally for small sliders for lateral core pulling.
diagonal bracing12Fixed by spring screw and guard. Strength of spring is 1.5-2 times the weight of slider. Applicable to upward and lateral core pulling.  
diagonal bracing13Fixed by spring guard, Strength of spring is 1.5-2 times the weight of slider. Applicable to big slider, upward and lateral core pulling.

Connecting method of slide insert

How slider head insert connected is controlled by end product. Different end products have different connecting methods.

The slider head insert connected methods details:

DiagramDescriptionDiagramDescription
diagonal bracing14Integrated structure
Applicable to situations of large cores, good strength.
diagonal bracing15Fixed by screw.
Applicable to situations of cores, round, or cores are small.
diagonal bracing16Fixed by screw.
Applicable to situations of square cores/small or medium cores
diagonal bracing17Fixed by screw.
Applicable to situations of square cores/small or medium cores

Guide form of sliding block

In the slide guiding, the slider must be smooth and stable so that no stutters or beats, which will affect the aspects, like quality and service life of mold. (Link for the specifications of platen)

The common sliding guide forms are shown in the figure below.

DiagramDescriptionDiagramDescription
diagonal bracing18Integrated manufacturing  mode, hard to manufacture, applicable to small mold manufacturing.diagonal bracing19Clamping plate ¢ral rail mode.
Applicable to situations of long slider and high cavity temperate.
diagonal bracing20Rectangle platen. Easy to manufacture. Fine strength, wide range of application, the specifications of platen is on standard parts list.diagonal bracing21“T” groove inside the slider.
Applicable to situations of small space, like slide inside the slider.
diagonal bracing22Applied “7” shaped clamping plate. Easy to manufacture, good strength. normally fixing with pinhole together.  diagonal bracing23Inserted “T” groove, good stability, hard to manufacture.

Calculation of tilt slider index

Due to the undercut surface of the end product is tilt, so the move direction of slider should follow the direction of end products’ undercut surface, otherwise it will cause damages when pulling the end product.

When the angle situation between the slider core pulling and the parting surface is called the slider pulling direction moving-die.

Shown as pic:

Situation when the angle between slide core pulling direction and parting surface is slider  pulling direction fixed-die.

Shown as below:

master mold runner slider

application features:

Undercuts forming  on the side of master mold

Marks are allowed on the appearance

Medium slider forming area

Shown as below:

Undercut forming on the side of master mold. No marks allowed on appearance. Need to switch to master mold runner slider.

Master mold tunnel block shown as below:

gst mold opening:

second mold opening:

second mold  Designing tips

a. Thickness of top clamping plate H2≧1.5D (D – diameter of large tie rod; hyperlink of large tie rod diameter calculation, three play mold large tie rod calculation; H2- thickness of top clamping plate).

b. Depth of pulling block inserted on the top clamping plate H≧2/3H2

c. There should has taper on SPRUE BUSHING head to fit for clamping and should be on the top clamping plate to avoid brush nozzle on the molding machine separating from SPRUE BUSHING and then result in brush, which is inconvenient to take out and affects next injection.

d.when pulling block inside the cavity plate, should reduce material.

e.The wearable plate should be 0.5mm higher than master mold plate to protect the taste mold plate and support the support pulling block to prevent it from distorting due to the external force.

f. Small pull rod limit stroke: S≦2/3H1 assist with mold clamping. (H1 – height of the slider)

g. It is best to have fixed block on the front of pole, easy to adjust and processing, consist three point bearing, increase the strength of pulling block.

h.To make the wearable block assemble smoothly,  E point should on the right of D point. Shown as below:

I. When assembling slide base and pulling block, need to notice about the relationship between size B and B1, it shoulbe B>B1, while in order to  assemble  smoothly, can also dig through the rear mold located after the slide base.

Dos and don’ts & calculation formula of double “T” groove

Shown as above:

S3=H*tgγ;   

(H – the decreased height of slide block which is the small pull rod stroke; γ – the angle of pulling block)

S2=δ2*cosγ;   

(δ2 – the space between pulling block and slide block, normally is 0.5mm)

S=S3-S2=H*tgγ-δ2*cosγ=(H*sinγ-δ2)/cosγ; 

 (S — horizontal moving distance of slide block)

S4=δ1/cosα;  

(δ1 – slider insert and space between sliders;α -tilt angle of slider insert)

S1=(H*sinβ-δ1)/sin(α+β); 

(β – space between grooves,normally is 0.5mm;S1- distance of slider insert out from the undercut)

Dos and donts:

a. Assemble requirements: assemble the slider insert and inclined insert hole, it should notice the relationship between the size A and A1, should be A>A1.

b. Double “T” groove tolerance, shown as below:

Case of Assemble matters

Die sketch

pic above :

Slide insert can be put inside the core insert without problems, required S1>S or open the core plate.

  β=α+2°~3° (easy to open mold and reduce scratches)

H≧1.5D    H is diagonal brace pin matching length; D is diameter of diagonal brace pin)

Double “T” groove structure model:

Double “T” groove structure model:

Cavity explosive slider

applicable situations of explosive slide block

Generally, forming on the cavity side and large slider forming area, especially using slider when the cavity side is very deep.

Explosive slider as blow pic shows:

mold opening state:

Stroke calculation:

Shown in the pic below:

S=L*sinβ  (β- “T” groove angle;L stroke along the “T” groove direction; S –  distance of slide block horizontal movement)

H=L*cosβ  (H distance of slide block vertical distance)

Design tips and notices of explosive slide block

Shown as the pic on the right:

a.bottom wearable plate needs bevel, reduce loss between slide block and core plate, normally takes 1.5˚~3˚, assemble location be at the 3 / 4 of the center of gravity of the slide block.

  b.S1>S (S – distance of slide block horizontal movement)

c. the wearable plate on the back of slide block and should be 0.5 mm higher than slide block’s back.

e. The angle between block and grab hook γ> the wearable plate obliquity.

  f.β=α (β is “T” groove angle;α is lmit rod angle)

g. T – block should be longer and 10 mm higher than cavity plate.

h. Slide block head should have die screw, easy to group the mold. Need to take down when testing mold

i. Lock T-block screw should be vertical to T block.

j. The spring at the head, should calculate the weight of slide block.

k. The back of the slide block should be tool setting plane.

l. Both flanks of slide block should have limit groove.

m. The slide block head must have datum plane to provide convenience for grouping mold. The processing base level is normally over 8mm.

n. Explosive slide block must have shoulder (wings for fixing) to provide convenience for grouping mold and also a base level is necessary, cannot reduce the material)

The assemble location depends on the location of the gravity of slide block.

Dos and don’ts of Extra deep explosive slide block

the guide rod should assemble from the cavity plate

a、Cavity plate should be  embedded into the core plate,avoid the cavity plate outward lift, enhance the mold strength

b.wearable plates needed at the protruding side of cavity plate, avoid scratches, easy to adjust.

c. Other precautions are the same as above

Place ejector pin inside slider

Generally, for thick and deep products’ wall, the side of the wall has many core pulling holes. The core pulling force is strong, so when moving the slide block, the product might be distorted or scratched. To avoid these happening, we need to place the ejector pin inside the slide block to stop the distortion or scratches.

A. Place ejector pin inside slide block (example 1)

B. Two common ways to place the ejector pin inside slide block, shown as below:

 Delay slider

1. The outside product pulling force is strong, avoid distortion.

2. Use delay slider to operate forced demolding.

The pic below is water pipe and water pipe delay diagram:

1st mold

 Finishing state after 2nd mold opening

oblique slider

1. Application range of oblique slider Normally applied in the products with slider structure, at the same time, along the slider’s direction, the end product also has undercut, which indicates that we can apply oblique slider.

note:

Pic on the right is typical case of oblique slider

2. Oblique slider diagram:

3.internal slider

(1) use boss form (seen as below)

Use the form of diagonal brace pin (as shown below)

In the figure above

S1 = S + 1mm above(S, undercut distance;S1 distance of slider moving

S2=S1/cosβ         (S2, horizontal distance of slider;β obliquity of slider)

S2=S3=(H1*sinα-0.5)/cosα  (H1, relative vertical height; obliquity of diagonal brace pin       ≦25)° 

γ=α+2°~3°

H≧1.5D    (D, diameter of diagonal brace pin; H, matching distance of  diagonal brace pin)

*Detailed dimension calculation hyperlink oblique slider calculation*

Calculation of core pulling force & strength checking

1. Calculation of core pulling force

After cooling, the plastic will be narrowing and shortening, including the die core and the other parts (like oblique tip, slider, insert etc)Therefore, we must consider the enclosed strength that end product impact on slider, stress state, see pic on the right

note:

F=F4*cosα-F3cosα=(F4-F3)*cosα

 F—core pulling force(N);

F3—F2 lateral component(N)

F4— core pulling resistance(N);

α—obliquity of de-molding. as α is normally low, so cosα=1

That is    F=F4-F3

But   F2=F1-cosα

F3=F2tgα=F1cosα*tgα=F1*sinα

F4=F2*μ=μ-F1cosα

So  F=F4-F3=μ*F1cosα-F1sinα=F1(μcosα-sinα)

F1——the enclosed strength that plastic on core (N)

F2—perpendicular to positive pressure on the surface of core(N)

μ—the friction coefficient between palstic and steel, normally is around 0.2

While F1=CLF.

The average circumference of core cross-section part which enclosed by plastic.

L—the distance of core part enclosed by plastic (CM)

F0—enclosed strength of unit area, normally 7.85~11.77MPA

Namely F=100CLF0(μcosα-sinα)  (N)

2. Diagonal bracing tip diameter checking:

The diameter of diagonal bracing tip is affected by many factors, like obliquity, length, and required de-molding distance. Thus, in designing, some parameters should be adjusted and matched to obtain the best result to make sure the slider to move smoothly. Calculation formula:

Note:P – maximum bending force on taper pin

L— bending moment

P1—core pulling resistance

H— distance from core pulling hole center to point A

α°—obliquity of taper pin

P2—mold opening force

From the pic we know:

P=P1/cosα (KN)

M curve=PL (KN)

Which is    M curve≦[σcurve]*W   (KN)

namely   PL=[σ curve]*W  (KN)

W—bending section coefficient

[σ curve]—permissible bending stress(for carbon steel – 13.7KN/CM2 (137MPA)

M curve—maximum moment on taper pin

Namely:     W=(πd4/64)/(D/2)= πd3/32=0.1d3

0.1d3=pL/[σ]=PH/([σ]cosα)

0.1d3=pL/[σ]curve=PH/([σ]curve cosα)

D=3√(ph/0.1[σ]cosα  (cm)

D=3√(ph/0.1[σ] curve cosα  (cm)

3.size of pulling block section checking

The size of pulling block section checking is as same as the calculation of diagonal bracing tip. It only needs to alter the last step. Formula:

W=bh2/b

When     b=2/3h,    W=h3/9

h3/9=pL/[σ] curve =PH/([σ] curve cosα)

H=3√9PH/([σ] curve cosα)   (cm)

When     b=h,       W=H3/b]

H=3√(6ph/[σ] curve*cosα)  (cm)

h—long side of puling block section(cm)

b—short side of pulling block section(cm)


2023年9月18日星期一

高通猝不及防!3nm芯片突然宣布,外媒:果然留了后手


#百家新收益#

本文原创,请勿抄袭和搬运,违者必究

高通的旗舰芯片市场地位正在受到动摇,联发科这几年里快速崛起,已经连续12个季度拿下全球智能手机AP处理器第一名。今年第二季度联发科全球智能手机芯片市场份额占据30%,领先高通的29%。

不仅如此,联发科在高端芯片方面也完成了3nm的流片,预计明年量产。高通猝不及防,外媒:联发科果然留了后手。

3nm芯片时代之争

人们对数字化、智能化的需求不断增加,越来越多的设备和应用需要使用芯片进行计算和处理。在人工智能,数据中心等高算力场景,已经不局限于使用7nm,5nm芯片,而是不断研发出更先进的3nm芯片产品。

目前世界上第一颗3nm芯片已经搭载至终端产品了,在苹果最新发布的iPhone15Pro和ProMAX机型中便采用业界首颗3nm芯片A17Pro。

根据苹果的介绍,这颗3nm芯片内含190亿个晶体管,拥有六核CPU,16核神经引擎,图形处理器性能提升20%,CPU运行速度提升10%。

这毫无疑问是全世界最先进的芯片,且不说苹果相较于上一代芯片“挤牙膏”的操作,就A17Pro芯片本身而言,放在当前任何一个使用场景都是最顶尖的,因为它采用的是台积电3nm工艺。

作为全球第一大芯片代工厂,台积电的工艺良率,制程水准始终领先三星,苹果获得台积电首批3nm产能,自然可以率先将3nm芯片终端产品推送上市。3nm芯片时代之争已经开启了,各行各业都会因此赋能,更多的3nm芯片也在赶来的路上。

由于苹果A系列芯片不对外出售,所以非苹果用户只能从其它手机厂商获得3nm芯片体验。

论竞争,高通和联发科才是同台竞技的对手,苹果生态独立,手机厂商要想获得最先进的3nm芯片供应,只能与高通或者联发科合作了。那么这两大巨头的3nm芯片进展如何呢?

联发科3nm流片

高通的旗舰芯片在移动设备市场上拥有很高的地位。其骁龙系列芯片一直是全球移动设备市场的领先者。所以高通是不会缺席3nm芯片时代竞争的。

目前可以预测的是,高通3nm制程芯片会命名为骁龙8Gen4,同样会在明年发布。有消息称,高通3nm芯片会瓜分台积电15%的产能,为确保产能,高通将回归三星代工,让台积电,三星这两家巨头共同为高通生产3nm。

高通3nm处于怎样的发展阶段,是否研发成功,或投入流片等等都尚未可知。相比之下,联发科传来3nm流片成功的消息了。

据联发科正式宣布,首款采用台积电3nm工艺的天玑旗舰芯片开发十分顺利,已经成功流片,预计明年量产。

联发科成功流片3nm工艺的天玑旗舰芯片是一个重要的里程碑,这意味着该公司正式进入了3nm工艺时代。3nm工艺比目前的5nm工艺更加先进,可以在同样的面积内容纳更多的晶体管,从而实现更高的性能和更低的能耗。

一款芯片到了流片阶段,相当于制造厂商已经开始使用实际的制造工艺在硅片上生产芯片。在这个阶段,芯片设计师将会验证设计的正确性和性能,并对芯片进行全面测试。

如果测试结果符合预期,芯片将会被用于实际的产品中。完成流片,距离量产上市也就不远了,进展顺利的话,明年春季或许就能看见搭载联发科3nm芯片的终端产品了。

联发科的逆袭

在2020年之前,联发科还是一个名不见经传的二三线芯片厂商,和风头正盛的高通比起来,几乎没有什么影响力。彼时的联发科在高端芯片市场上表现不如高通等知名厂商,甚至联发科还没有自己的高端芯片产品,长期专注于中低端芯片市场的策略。

相对来说,联发科的中低端芯片产品性能稳定、功耗低、支持多种通信技术,并且价格相对较低,非常适合二三线手机品牌等客户的需求。

可毕竟是中低端产品,知名度终究是有限的。直到联发科抓住了5G芯片市场的需求,推出多款极具性价比优势的芯片,此后的联发科一步步从中低端向高端迈进,7nm至4nm的芯片产品接踵而至。

国内手机厂商也开始多元化选择,联发科的逆袭开始了。在全球智能手机市场上,联发科的出货量越来越高。

根据调研机构Counterpoint Research公布的数据显示,今年第二季度联发科全球智能手机芯片市场份额为30%,超过高通的29%。

从2020年第三季度以来,联发科已经连续12个季度领跑了。也就是说,在过去三年联发科始终是超越高通的存在,就连高通的旗舰芯片市场地位也要联发科动摇了,还率先高通一步完成3nm流片。

估计高通猝不及防,曾经二三线不起眼的芯片厂商,现在已是世界第一,外媒:联发科果然留了后手。多年的蛰伏换来一鸣惊人。

随着明年联发科3nm芯片产品的登场,恐怕在未来的3nm芯片时代竞争中,联发科会更加耀眼。